I heard that Class C HSS might undergo some cracking when galvanized.

Any published literature on this topic?

thanks
 
Replies continue below

Recommended for you

At the InterGalva Conference in Italy in June some informqtion will be presented on cracking issues with galvanized coatings.

Cracking of Large Steel Structures (the Designer’s View):
Prof Dr M Feldmann (University of Aachen RWTH, Germany)

Current Knowledge of the Cracking of Steels During Galvanizing – A Synthesis of the Available Technical Literature and Collective Experience:

Tom Kinstler (GalvaScience LLC, USA)

Here are some picture of ASTNM A500 C HSS that cracked during galvanizing.

117341857.jpg

117341853.jpg

117341843.jpg

117341841.jpg

117341831.jpg