I have a situation, where I need to connect a Fiberglass 3" 3000# from a Well Head Christmas Tree to Existing 4" 300 RF Flowine which is also obviously coming from another well!

I have no Idea how to couple 3" 3000# Line to 4" 300# Line.

I never worked in FRP pipelines before,

So there is also another question is 3" 3000# FRP flange is RF or RTJ?

Can anyone help me out, here!!!

Thanks in Advance!!!
 
You are truly overthinking this. Add a 3" API 3000 flange to the FRP. Build a spool with a steel 3" API 3000 flange on one end, weld a 4X3 concentric reducer to it, finally weld a 4" ANSI 300 flange on the other end. It really is that easy. If the bolts are too hard to get to, add a 3 ft pup to either end (the 3"inch might be a few dollars cheaper, but hydraulically it doesn't matter).

David Simpson, PE
MuleShoe Engineering

"Belief" is the acceptance of an hypotheses in the absence of data.
"Prejudice" is having an opinion not supported by the preponderance of the data.
"Knowledge" is only found through the accumulation and analysis of data.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top