Jun 2, 2006
688
I have a project where a customer is interested in using aluminum to build a differential housing instead of cast iron. All my past experience is in cast iron - as far as bearing fits, working stresses, machining, casting, etc.

The goal is to design a stronger/stiffer housing than the OEM cast iron unit. The aluminum option is intended to save weight.

What material should I consider for my aluminum casting? What is the most reasonable casting process for producing under 200 units? I intend to contact the bearing manufacturer for housing fit recommendations.

Any tips appreciated.

David
 
Replies continue below

Recommended for you

Ford 9"? You can buy reliable Ford 9" aluminum differentials off-the-shelf.

57012-1.jpg
 
Will this be to compete in the marketplace with products like Heidt's 9" Ford-based IRS?
 