Anyone know the friction coefficent across two metal surfaces that are painted and then bolted together?
Currently I'm using 0.16 which is the same for lightly oiled surfaces, but does anyone know any better?

Cheers,

Andy
 
Replies continue below

Recommended for you

The application and specific coating type vary the coefficient factor. For structural applications, refer to AISC-ASD, 9th Edition, Appendix A for further info.
 
Andy,

Friction varies so much, even for the "same" conditions. It is impossible to identify a single value for friction coefficient, so I question why anyone would publish a single value rather than a range. Ranges for "lubricated" metal parts can range as low as ~ 0.05, but my experience has been that polymers (without PTFE or other low friction constituents) should not be below ~ 0.1. Thus, I would use 0.1 to be conservative.


Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Super, thanks Cory. Being in the UK I don't have access to the AISC-ASD data.