Does anyone know if there is a correlation between Plain Strain Fracture Toughness (K1c) and Impact Toughness (results of a Charpy impact, or Izod test)?

Crux of this question is that I'd like to be able to predict as far as possible the K1c for a material that I only have Izod test results for.
 
Replies continue below

Recommended for you

thread367-168382

thread330-65956

thread330-60518

thread330-24020

thread330-128281

thread330-67872

Regards,