Fracture Toughness (KIC) value for 2014-T6 1

Status
Not open for further replies.

shibbyz

Mechanical
Feb 15, 2013
4
Does anyone have any fracture toughness data for 2014-T6 sheet? Any information will help.

Thanks
 
Replies continue below

Recommended for you

DOT/FAA/AR-MMPDS-01 Metallic Materials Properties Development and Standardization, Table 3.1.2.1.6. Values of Room-Temperature Plane-Strain Fracture Toughness of Aluminum shows 22 ksi in0.5 in the L-T orientation.
 