Hi,
I have conducted impact testing on my NbSi alloy at RT which is very brittle. What could be the relevant formula to evaluate the fracture toughness (stress intensity factor) of the material? I have few relations to calculate stress intensity factors but it's not clearly explained it can be used for brittle material as well. What other properties can be evaluated from the available data from the impact testing.
thank you
Vinston
I have conducted impact testing on my NbSi alloy at RT which is very brittle. What could be the relevant formula to evaluate the fracture toughness (stress intensity factor) of the material? I have few relations to calculate stress intensity factors but it's not clearly explained it can be used for brittle material as well. What other properties can be evaluated from the available data from the impact testing.
thank you
Vinston