where can i get the information about the fracture strength or Ultimate Tensile Strength of CVD SiC.
 
Replies continue below

Recommended for you

Notes from an SPIE short course by Roger Paquin lists CVD SiC with a fracture strength of 595 MPa, a Young's modulus of 465 GPa and a Poisson ratio of 0.21. Material is considered for use in sophisticated optical structures.
 