My understanding with regard to forgings to ASTM A694 is that the material must undergo significant work, usually reduction of 4 to 1. However I find that some companies certify to ASTM A694, material such as seamless pipe (API 5L X52) that has been hot worked to form fittings such as equal tees. Is it valid to certify this as a forging to ASTM A694?