Hello,

Could you help us to find out our seperator material related specifications? It can be seen below chemical composition.

DIN 40NiMoCr10 4 is a specifications that i could find closest specifications.

Is there any welding recommendations for this material?

Best Regards,

10.09.2019_xyrjw8.png
 
Replies continue below

Recommended for you

This looks a little like a 48xx steel.
Is it real thick?
These steels are usually used either for very t hick parts or for low temp service.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 