Can you please tell me where I can find pressure/temperature rating charts for 316L forged fittings?
 
What kind of fittings?

For flanges refer to ASME B16.5

NozzleTwister
Houston, Texas
 
Use ASME B16.5 instead of 1952 and 1963 codes. Even mechanical engineering standards have changed a lot since 1963. Use B16.11 for welded and threaded fittings.
 