Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Forcemain - Material and Cost 3

Status
Not open for further replies.

jhayesmiller

Civil/Environmental
Joined
Jan 28, 2009
Messages
4
Location
US
I am gathering some back ground information for what is required to install a 2" diameter forcemain.

What material is best suited, pvc, pe? And can anyone give just a rough idea of cost/foot assuming:

3' cover, mid-atlantic state, no rock, on-site private system, there really aren't any conditions forseen that would complicate the installation... just need a rough idea to start from.

Thanks!
 
For 2", DR-9 HDPE. Maybe $8 a foot for a big job.
 
OK, I had been thinking more in the range of $15-$20 foot (about 3000 feet total). Could you tell me, do they weld the pipe joints or are they mechanically restrained or thrust blocks used? what is the most common for a small line such as this?

Thanks
 
You may perhaps be interested in the information at and/or while I don't know exactly where you are/what is involved the “Ten States Standards” for wastewater accessible at [If this is an ordinary domestic sewer system forcemain in an otherwise gravity system, note in the latter that section “49.1 Velocity and Diameter…” says, “The minimum force main diameter for raw wastewater shall not be less than 4 inches (100 mm).”]
 
It would be easiest to use 2" (I like SDR 11) HDPE pipe. It comes in a roll of probably at least 1000 ft (maybe more). You can install via horizontal directional drilling without even having to dig a trench. Very easy and the cost should be about the same or less as open trench for a 3000 ft project.
 