Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

[For filler metal] Same AWS classification but different manufacturers.

Status
Not open for further replies.

Koodaehan

Petroleum
Joined
Mar 22, 2014
Messages
2
Location
KR
Dear Sirs.

Good day.

Please kindly refer to below my questions.

1. Now i have a Qualified WPS but it's designated only type(E8016-C1) and Manufacturer(Kobelco).
2. But as missed order from company that arrived diff manufacturer(Chosun) welding rods(but same AWS classification : E8016-C1)

So do i have to PQR again? Is it essential variable? or Non-essential variable situation?
Please kindly guide us for this matters.

Thanks in adv.


From. Koo, Daehan-Newbie.
 
koodaehan,
If you are talking ASME IX then no problem at all with what you propose,
Regards,
DD
 
As DekDee said, for Section IX it is not a problem. If you are working to some of the EN welding specifications you may want to look very carefully at them since they often require a new PQR with change of manufacturer. They do make exceptions for solid rod but I don't recall the exceptions carrying over to the SMAW process.
 
Note that ASME does not discriminate as per Mfr or
Country of origin
 
It depends; if the WPS specifies a specific manufacturer or a specific trade name, the WPS must be revised as a minimum.

Best regards - Al
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top