Aug 9, 2001 #1 48660544 Aerospace Joined Aug 9, 2001 Messages 8 Location DE Does the possibility exist that the Flexible silica Aerogel Blanket is transparent?
Feb 28, 2002 #2 barpaul Materials Joined Feb 28, 2002 Messages 3 Location US How flexible do you want it ?. The silica aerogels are known as a brittle material. It can be made flexible (resilient) if doped with organic precursor. Upvote 0 Downvote
How flexible do you want it ?. The silica aerogels are known as a brittle material. It can be made flexible (resilient) if doped with organic precursor.