Hi,

I am looking for a suitable flexible, plastic product for making a closed extrusion for us which would be used outdoors (outdoor, flexible, plastic, extrusion)
We would like flexibility since it allows us to form extrusion around curved architectural features

Ideally, we want:
1) Optical clarity > 88% for 1/16" THK wall
2) Flame rating UL 94 HB or greater
3) UV rating UL746C f1
4) Operating temperature -40 C to 85 C
5) Temperature rating (RTI electrical) UL 746 > 90 deg C

Note that we are flexible on some requirements so we don’t have to have all our requirements exactly met

Plastic would need to be clear since we are inserting our light product within the extrusion.

Please let us know if you know of any suitable plastic which could meet our needs

Currently, we use polycarbonate for our extrusion, but with a flexural modulus of over 2200 MpA, it is too stiff
So far, the best option we found was a copolyester material from Eastman (Tritan GX 100) which has a flexural modulus of 1480 MPa

Cheers, Greg
 
PVC might work well for you. It can be made as flexible as you like by adding plasticiser.
 
I've looked at flexible PVC. The problem it has is that visibility is low, and haze is high, so it seems it would not meet our visibility requirement.
If you know of a flexible PVC which would meet our requirements, please let me know
 
PVC can be very clear. You just have to find the right supplier/processor. I can't really help with that. Are you the extruder? You may also want to consider other processing possibilities like vacuum forming from sheet.
I'm pretty sure that rope lights I've seen are extruded PVC.
 
PVC is the obvious choice. As mentioned, it can be very clear (think identical look to a PET botttle as some such bottles are in fact made of PVC). Also PVC is inherently flame retardant and inexpensive. See for example this link to extruded PVC clear and tinted film.


Chris DeArmitt PhD
President - Phantom Plastics LLC

Consulting, ideas and training on plastic materials
 
Thanks for the information

I will further investigate flexible Clear PVC.
One issue we may have with this material is that it may be too flexible which could cause issues when material is extruded,and we want to retain consistency of shape
Our extruded profile is to be similar to rectangular tubing with aspect ratio of 4:1 or greater with approx 1/16" wall thickness

Please let me know if you know of any more rigid plastics which meet our requirements.
So far, Tritan Copolyester (GX 100), and Butyrate such as Excelon CAB, are best options I have found
 
Unplastisized PVC is pretty stiff. Look-up clear PVC pipe. So, as I said before, you can get it as stiff or flexible as you like. However, I suspect you want an intelligent material, which knows when you want stiffness and when you don't.
 
PVC has similar stiffness to the materials you said you like.

Chris DeArmitt PhD
President - Phantom Plastics LLC

Consulting, ideas and training on plastic materials
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top