Flaring tool for nylon

Status
Not open for further replies.

peterlee

Mechanical
Aug 23, 2007
4
Hello,

I am looking for a flaring tool to be used on 3/8" OD, 0.050" walll thick nylon tubing. Does anyone know of such a tool? Is any heat source required in forming the flare on the nylon?

Rgds,
Peter
 
Replies continue below

Recommended for you

If this is a fluid or pnuematic line, consider using ferrule or instant fittings instead of trying to flare the line. If you heat the line to less than its melting point and flare it using an ordinary flaring tool, you can no longer be sure of its mechanical properties IE: the tube may burst or even break at the flare.
 