Hello - I am after some help.....

We have a customer that has requested a replacement vessel for one we previously supplied a few years ago. At that time the vessel used BS4504 PN16 flanges for nozzle connections. However the new BSEN1092:2002 has superceded BS4504, and these PN16 rated flanges have a reduced PT rating meaning I am unable to supply a design that would suit the required connection dimensions and the pressure/temp rating - am I correct in thinking this, or have I overlooked something??

Flange material is ASTM A182 F316L. Pressure 10 Bar.G. Temperature 200degC. Design is CAT III to the PED meaning third party appraisal by Lloyds.

Regards,
Lee
 
Hi Fawkes,

Thanks for your response - the dual rating aspect is something that would be useful, and I'd never considered.

The flanges are DN100 - so the PN40 rating does not apply unfortuately.

I asked our flange suppliers and they told me that the flanges are still marked with BS4504 anyway and that if we wanted flanges to EN1092-1 then it would cost us more and take longer to get!! Also, PD5500:2006 section 3.8.1 b) states that flanges must comply with an appropriate Bristish Standard, BS1560 / BS4504 / BS EN 1092 - I thought 1092 replaced BS4504 from 2002??

The other thing that puzzles me is that the material group 13E0 seems to be a 316L equivalent (1.4404), but flanges made from this group have much higher PT ratings than the ASTM equivalent - am I missing something here?? If not, then I'd just ensure that we purchase and use flanges of this group when we design the vessel - but the design code would need to be PD5500 and not our usual ASME.