Any innovative fireproofing products out there other than the usual spray on fireproofing, cast-in-place concrete encasing, or a constructed protection boxing ?

thank you.
 
Replies continue below

Recommended for you

Another option is intumescent paint. Commonly used for architecturally exposed steel.
 
i have heard somthing about it. should i trust it. how good is it?

Thank you.
 
As the result from lab testing, the intumescent can resist fire about 2 hours
 