Does anyone know of a viable alternatives to grafoil packing or gaskets to make a valve fire safe? I am looking to see if I can get an oring type seal (shaft in a bore) that is self energizing to act as a fire safe seal.

I have very little experiance in this area and may be dreaming of the impossible, but any suggestions will help.

Thank you in advance for your comments.
 
BigMac23,
you might try, for example, to see the following:


They've got solutions for very low temperatures, may be they have something for high temperatures too... even if I feel you should look at ceramic fibers more than at elastomers and plastics.

So I'd suggest to look for "HEPHAISTOS®" packing into the Latty website:


Hope this helps, 'NGL
 
BigMac23,
To make a valve fire safe,there are many things to deal with. Besides the materials of packing and gasket will be choosen the graphite or 50%graphite+50%316stainless steel, the capability of valve's seal or the leakage after fire is also worth the whistle. So the structure of valve-body would be disposed in factory.
 
Is it necessary to include the thermal expansion in the design? The temperature changing may be so sudden.
 