Hi all friends,

I need to learn something about finishing.Could you give some information about this sentence ?
" The bore should be finished by techniques known to produce approximately 12rms "

Thanks for your interest
 
Replies continue below

Recommended for you

If this is a machined surface finish then it represents roughness in micro inches assuming imperial units. RMS = root mean squared average. 12RMS is fairly smooth and would typically be obtained by grinding.
 