Jul 13, 2020 #1 Castroii Mechanical Joined Feb 20, 2020 Messages 4 Location NG Dear Professionals, can EH14 SAW filler wire be use with ASTM A36. What do you all think?
Jul 13, 2020 #2 Guest Ask your local Lincoln or similar sales rep. Ask them about flux as well. "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
Ask your local Lincoln or similar sales rep. Ask them about flux as well. "Everyone is entitled to their own opinions, but they are not entitled to their own facts."
Jul 15, 2020 #3 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US Have seen it used in the past, mainly when impact testing was required for the A-36 material. Upvote 0 Downvote