Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Filler material chart SS HELP!!! 1

Status
Not open for further replies.

sirexer

New member
Aug 6, 2003
2
Hello. This is my first post here. I'm a recent college graduate who is working for a manufacturing company. So much to learn, so little brain I have.

They want me to check the filler mat'l chart and fix it. I haven't had much luck finding the correct filler mat'l when diff. SS are being welded.

I am trying to find a reference chart when stainless steel is base metal without having to buy AWS books. Can you guys point me to a website where I can find a such information? or anybody would want to share?

Thank you all in advance.
 
Replies continue below

Recommended for you

Thank you all for great help. I really appreciate it.
If I'd make a purchase on AWS product, which one would be the best choice? Suggested/recommended filler mat'l is my main concern of course. I'm interested in diff. base metal(SS) welding especially.

Thanks again.

Fresh out of school, having hard time calling myself an engineer yet.
 
Contact any (all?)of the welding electrode suppliers - many have selection tables within their brochures.
 