Jan 23, 2013 #1 pinoyce Civil/Environmental Joined Jan 9, 2013 Messages 13 Location US How do you guys test fillcretes? My cap always comes off even though the temperature is right.
Jan 23, 2013 1 #2 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US Depends on the expected strength. If in the 500 psi range and below, don't cap them....just sand the ends flat on medium to coarse sandpaper. Upvote 0 Downvote
Depends on the expected strength. If in the 500 psi range and below, don't cap them....just sand the ends flat on medium to coarse sandpaper.