Figure UG-29.2 - ASME VIII DIV.1.
If I have a value below the last curve Arc=0,390*Do, do I have to consider it equal to 0,390*Do whatever L/Do is? thanks
 
Answer: consider 0,390*D.
See interpretation Number : VIII-1-89-121
 