If a ferrite count were to be conducted on a 316ss weld what would be the acceptance criteria for the parent metal, weld and HAZ?

Geoffrey D Stone FIMechE C.Eng;FIEAust CP Eng
 
Normally, for austenitic stainless steel weldments you want to have a minimum ferrite number of FN 4 to avoid solidification cracking. Regarding base metals, the ferrite content should be as low as possible. I have seen ferrite numbers for austenitic stainless steel base metals vary from 1-4 depending on product form.

Acceptance criteria for corrosion tests and ferrite content should be based on service application. I would go back and discuss with the Purchaser what their needs are and service duty.
 
I presume as welded (no anneal), but with or without filler metal?

The base metal value should be low, limits of 0.5% are used in some process applications. In some cases 1% would not be bad.

I would expect the weld to be what ever the weld was designed to be. If the aim value was 4%, then 2-6% would be reasonable.
Why not measure magnetically?

= = = = = = = = = = = = = = = = = = = =