Our company, in an associated field, produces a byproduct of ferric chloride solution containing approximately 4.5 ounces of copper per gallon. I have been told this solution may be used in the copper mining industry. Any information or users is appreciated.
 
you can always plate the copper out and sell the metal.

 
Contact companies that recycle etching and plating solutions.

It depends a lot upon your solution volume, location & transportaion costs whether you should recycle this yourself or send it to a professional recovery company. In the USA, you could use Phibro-Tech to extract the copper and return the ferric chloride (etchant?).

Phibro-Tech (they recover & sell both chloride and copper solutions):

If you want to try electrolytic recovery of the copper, US Filter sells an Electrolytic Heavy Metal Recovery Systems (among other things):

Among the many other mfrs. of electrolytic recovery units are:
Electrolytic Recovery Equipment
Canadian Finishing Systems Ltd
Precious Metal Processing Consultants Inc
Recovery Engineering & Sales Co Inc
 