This is a product I have come across in working on existing school renovation projects, particularly in the upper Midwest, that can be difficult to find information on. Several posts throughout the years on this web site have asked about it with little or no response. I believe it has not been used in years, in fact in my 30 years of structural work I have only come across it twice, so I thought I would post the location below where you can find some information on this. I hope it can help you out if you run across it.

 