Hello all, I'm trying to find some specification on an Italian print note.

The treatment calls out for Fe/AC8 per UNI 3740-6. As I read the spec
Fe is: is base metal
AC is the chemical anti-corrosion coating, made of chromates metals and polymeric organic binders.
8 is the nominal thickness of 8 micrometer (extraordinary class) with a minimum specific mass of 32 g/m2.

Does anyone know a cross reference or perhaps explain what I'm looking at?

Regards,

Chuck
 