Does anyone have any experience with casting of steel with 3% Si (C<0.04%)?
I'm interested in feeding behaviour, can it be flame cut, what thermal treatment is normaly required?

Thanks for helping me out,

Mik
 
Do you mean that you wish to melt pure iron with 3% Si,with very low carbon? It should be brittle I suppose, You can use knock off risers/feeders. Hence no need to flame cut the gates and risers.

Interesting application,what is it used for and will there be any machining? I plan to process a small quantity out of curiosity perhaps tomorrow.

I shall then share a few more experiences. As the metal is low in carbon,most of the silicon addition might be consumed as a degasser. You may need to compensate for this loss.

Hope this helps.
 
This isn't steel, it is ferroSilicon. Jokes aside, this is the standard silicon steel for transformer laminations. About 3.8% Si and <0.02% C. It is ductile enought to roll fine. It is so soft that it hot rolls very fast.
I am not sure about shrinkage. It should flow well.
You will need a deoxidizer so that you can control Si recovery and hit the desired level.
What finishing are you going to do?

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 
I don't know the application, but I suspect they want to draw a wire from this material.