gearman1234
Mechanical
WE have one appliocation for steering shaft for material handling equipment. Due to difficulties observed in shaping blind splines in 4140 shaft ( H/T to 28/32 HRC) we are changing it to broaching one end ( 3 inch long) and welding it to the other long end ( about 13 inches long).
My main concern is the fatigue properties of this welded joint. I do not have any information about the torque and no of life cycles.
Does any body has any information about the fatigue properties of such an application when a welded joint is used?
My main concern is the fatigue properties of this welded joint. I do not have any information about the torque and no of life cycles.
Does any body has any information about the fatigue properties of such an application when a welded joint is used?