F928 Mesh

Status
Not open for further replies.

ooox

Structural
Jun 22, 2009
95
Greetings all,

Anybody know the cross sectional area/m width for a F928 mesh? This would be for both the longitudinal and cross bars.

Many Thanks
 
Replies continue below

Recommended for you

nineninenine,
I take it that you know the F designation is not in use anymore. But if you are talking about the old 450 MPa fabric designations, F928 has 9 mm wires at 200 centres in one direction (318 mm^2/m) and 8 mm wires at 250 centres in the other direction (201 mm^2/m).
 
Thanks Hokie,

Its for a refurb dating back to 1992 so I'm aware that the mesh is no longer used.
 
nineninenine

AFAIK up to '95 there was either F92 or F918.

F92; 9 dia @ 200 crs EW G450
F918 9 @ 100 & 8 @ 200 crs, G450
 
It wasn't very common, but F928 was available at one time. Listed in the 1976 Reinforced Concrete Design Handbook, but not in the 1989 edition.
 
apsix,

I don't actually know that it was ever made, but it does appear in the 1976 C&CAA Handbook, pg. 152. At one time, the mesh folks made a big thing of saying they could customise fabric to almost any specification.
 