Hi
Can anybody advise me on possible applications for the F43 filler on ASME boiler and B31.1/B31.3 applications;
- SA-213-TP304H to SA 213-T22
- SA-213-TP347H to SA 213-T22
- SA-213-TP321 to SA 213-T11
- SA-213-TP321-H to SA 213-T22
- Tube to Tubesheet weld. SA-213-T22 (tube) to overlay Inconel (Tubesheet)
- P8 attachment welded to carbon and low-alloy tubes.
(problems with failures of the welds tearing into the tube instead of failing on the attachment side.)
If other filler is recommended what are the possible advantages?
Can anybody advise me on possible applications for the F43 filler on ASME boiler and B31.1/B31.3 applications;
- SA-213-TP304H to SA 213-T22
- SA-213-TP347H to SA 213-T22
- SA-213-TP321 to SA 213-T11
- SA-213-TP321-H to SA 213-T22
- Tube to Tubesheet weld. SA-213-T22 (tube) to overlay Inconel (Tubesheet)
- P8 attachment welded to carbon and low-alloy tubes.
(problems with failures of the welds tearing into the tube instead of failing on the attachment side.)
If other filler is recommended what are the possible advantages?