Can anyone tell me of any agents of Bosch that supply extruded aluminium in the North of England?

Thanks,
Paul
 
Replies continue below

Recommended for you

Try:
Almaco ( Selby) 01757 705979
Capalex (Cumbria) 01946 811771
Amech Engineering (Darlington) 01325 488884
MK Profiles Systems (Preston) 01772 202551

I don't know about them being Bosch agents though.
 
pclegg25

Not sure about the Bosch connection ??? but contact Eltheringtons (Stockholders & fabrication...Hull) 01482 320336 who can maybe help you out.
 