Dear all,
We have CS vessels and tanks require internal epoxy lining. When equipment arrived at site, found the lining on the face of flange was damaged and needs to be redone.
Questions from field contractor is: Is it necessary to line on the face of flange? They claimed it is not required.
Anyway, if it is deemed required,
(1) how to check if the epoxy lining surface is good for gasket seating? It can not be circular laid like metal, so not knowing what kind of surface preparation for gasket after lining.
(2). What kind of special gasket shall be used ? (demin water, slop oil, and other corrosive service) (304SS spiral wound which requires high seating stress may damage the lining). The connecting piping is galvanized.
Please advise if anyone has experience.
We have CS vessels and tanks require internal epoxy lining. When equipment arrived at site, found the lining on the face of flange was damaged and needs to be redone.
Questions from field contractor is: Is it necessary to line on the face of flange? They claimed it is not required.
Anyway, if it is deemed required,
(1) how to check if the epoxy lining surface is good for gasket seating? It can not be circular laid like metal, so not knowing what kind of surface preparation for gasket after lining.
(2). What kind of special gasket shall be used ? (demin water, slop oil, and other corrosive service) (304SS spiral wound which requires high seating stress may damage the lining). The connecting piping is galvanized.
Please advise if anyone has experience.