Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Explanation of DIN material codes

Status
Not open for further replies.

CMMehanicalWorks

Mechanical
Joined
Oct 11, 2013
Messages
4
Location
IE
After much experience working with ASTM material standards I am now assisting a german company for piping fabrication and Installation. One thing that I am finding difficult to understand is where the numbers in front of CrMo (and other letters) come from. Say for example 16Mo3 and x10CrVNB9-1 . Does the 16 and 3 have a direct reference to the amount of molybdenum or is it a different meaning altogether and where is the x coming from? . Also can you determine from looking at the material code the parts of chromium or moly. in a material as I came across tables that say materials fall into this category if they are 1/2 CrMo etc. Any help or references to books or websites would be a great help. Thanks to anyone who gives useful information.
 
The numbers sometimes have meaning for nominal composition, but most of the time they do not. Your best bet is to look them up in a reference such as the Worldwide Guide to Equivalent Ferrous Irons and Steels.

Aaron Tanzer
 
The designation of EN-materials is given in EN 10027-1.
There are different rules depending on the use, the alloy contnent,.....
E.g.
16Mo3 means an average C-content of 0,16% and Mo-content of 0,3% and no other major alloying element.
Different multiplication factors apply:
4 for Cr, Co, Mn, Ni, Si, W
10 for Al, Be, Cu, Mo, Nb, Pb, Ta, Ti, V, Zr
100 for C, P, S, N
1000 for B
This system mainly applies to steel grades if no element has > 5%.

X10CrVNB9-1 means an average of 0,10%C, 9%Cr, 1%V (I assume Mo is missing in your designation and the correct designation is X10CrMoVNb9-1)
X means that one element has > 5%.
The multiplication factor for all elements is 100.
The first figure is the average C-content.
Alloying elements are sorted in decreasing order. Generally, only the contents of the 2-3 most important enter in the designation.

All EN Grades are based on the rules of EN 10027-1.

 