bellows material B409 AlloyH (NO8810)
design temp specified 1200F
a exp.joint manufacture has come back with a design temp of 1000F, allowable stress 14,400 psi, elastic modulus 24.2E6 psi.
using MatPro (paulin.com) I was able to obtain a yield stress of 7,400 psi @ 1200F, elastic modulus 23.2E6 psi.
Not being a metalurgist of expansion joint professional I am curious if specifying the design stresses calculated with MatPro would be unrealistic.
Does any one have experiences with this type of material application???
Thanks
design temp specified 1200F
a exp.joint manufacture has come back with a design temp of 1000F, allowable stress 14,400 psi, elastic modulus 24.2E6 psi.
using MatPro (paulin.com) I was able to obtain a yield stress of 7,400 psi @ 1200F, elastic modulus 23.2E6 psi.
Not being a metalurgist of expansion joint professional I am curious if specifying the design stresses calculated with MatPro would be unrealistic.
Does any one have experiences with this type of material application???