HI ALL.
Two liquid ethylene storge tanks are to be inspected almost for the first time since begining of 80s. these tanks are constructed according to:
- CODE OF CONSTRUCTION: API 620 APP. Q, 6TH ED, REV. 2, 1978.
- OTHER SEPCS: SP-4615-41-2, 20-1...for insulation, piping...
the tanks are double wall of:
Inner tank MOC:shell: A-553, bottom/annular: A-553TP. 1/A353
Outer tank MOC:shell: A-283C, bottom/annular: A-283-C/A-283-C
Suspended deck :ALUM-5083-O.
what would be better inspction techniques, methodology, tools.
thanks
Two liquid ethylene storge tanks are to be inspected almost for the first time since begining of 80s. these tanks are constructed according to:
- CODE OF CONSTRUCTION: API 620 APP. Q, 6TH ED, REV. 2, 1978.
- OTHER SEPCS: SP-4615-41-2, 20-1...for insulation, piping...
the tanks are double wall of:
Inner tank MOC:shell: A-553, bottom/annular: A-553TP. 1/A353
Outer tank MOC:shell: A-283C, bottom/annular: A-283-C/A-283-C
Suspended deck :ALUM-5083-O.
what would be better inspction techniques, methodology, tools.
thanks