Hello my friends,
Today I heard new chemical name that I never heard before.
I investigated information and CAS number on the net and
I can not find anything.
Does anybody have any information about Ethyl santralite ?
What is the reaction ? What is ist used for ?
Thanks
 
Replies continue below

Recommended for you

Could it be that what you heard is ethyl centralite, CAS # 85-98-3, aka symmetrical diethyl diphenylurea, or carbamite, C17H20N2O ?
 
Thanks 25362
I don't know real word. May be there is mis letter or
wrong letter. Can It be used for rocket fuel ?
 
It appears as a (~6%) component of a propellant following, for example, USP 4,416,712.
 