Hi,
Can anyone out there shed any light on the above specification for this material.Any help would be greatly appreciated.Thanks Paul.
 
This is not a designation from any industry standard (ASTM, SAE, ISO, DIN, etc.). Ford Motor Company creates Engineering Specifications that use a similar type of nomenclature, ie, "ES" followed by a series of alphanumeric characters.
 