What is meant by API 5L X-42 Triple Stenciled Pipe? Is it X-42/46/52? Is single stenciled pipe available and would it have a lower maximum yield value? Is PSL1 vs PSL2 relevant to triple stenciled vs single stenciled?
 
Replies continue below

Recommended for you

Triple stencil means it could also be used under other standards like A333 Gr 6 pipe and at least one other.
 