Erosion and Corrosion Effect on Wear Parts

Status
Not open for further replies.

marklobo

Mechanical
Joined
Apr 11, 2001
Messages
30
Location
US
What does this body of knowledge have about material choices for resisting erosion damage from fluids that are also corrosive? Since erosion resistance typically has an inverse relationship to corrosion resistance, would a Rc 55 low alloy steel (e.g. Nitralloy 135) suffer from corrosion to the point of wearing out faster than 17-4PH H900 at Rc 45 when subjected to, say, high velocity "oil patch" water with sand, salt, H2S, etc?

I was surprised at the lack of a "hit" when I did a search about this subject here.
 
Have you tried:

Metal and Metallurgy engineering Forum
(16647 members)
forum330



"Do not worry about your problems with mathematics, I assure you mine are far greater."
Albert Einstein
Have you read FAQ731-376 to make the best use of Eng-Tips Forums?
 
You may also try a coating to help improve the erosion resistance. TMT Research in Smith River, CA offers some diffusion coatings for erosion protection on pumps and valves. Contact them if you are interested in that option.

 
>Since erosion resistance typically has an inverse relationship to corrosion resistance, <

I will concede that NACE stipulates "Do not exceed" hardness numbers, but that is the limit to which I agree with your premise. Stellite is more corrosion resistant to almost every process fluid than carbon steel, and harder, and more erosion resistant. Still you must primarily select an alloy that is corrosion resistant to the process fluid, or the corrosion products will likely be washed away. Back when I went to "sandbox 1 school" as a young pup valve engineer, they called this process KE-rosion-or combination corrosion/erosion.

If you address corrosion, you can control erosion by limiting velocity.
 