Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Equivalent BAC code for HL19PB70-6-10 2

Status
Not open for further replies.

zuccari

New member
Joined
Oct 16, 2003
Messages
2
Location
IT
Anyone know the equivalent BAC code for the Hilok HL19PB70-6-10?
 
Per Boeing D-590 Vendor-to-Boeing CR Index:

HL19PB70-6-10 = Pin BACB30FN-6-10 + Collar BACC30M6

The HL Part number is for a Hi-loc and Collar combination.
HL19PB-6-10 + HL70-6
 
Thanks rerig
Is the spec D-590 available somewhere?
 
It is a Boeing Publication.
It is online at My Boeing Fleet. ($$$$$)
We are low tech (less $$) and get a microfilm tape from Boeing Tech Pub Support.
 
hl19pb is a cad plate csk shr hi lok with collar hl86

sub fastener is s4931919-6-( ) as per matl sub manual.

Later ace
 
Available from huck corporation or interfast corp in Toronto, Ontario.
 
The 2024-T6 aluminum, threaded frangible collar correctly identified by rerig (HL70-6: is not the same as the 303Se tension-application collar identified by UG24U (HL86:
The "tension" application HL86 collar should never be used with shear head pins (such as the HL19: as the preload developed by the tension-application collar torque-off value can overstress, or even fail, the shear head pin.

The HL19 (as noted by UG24U) is a cadmium plated, alloy steel, 100° Flush Shear Head Hi-Lok Pin. The Hi-Lok Pin has a hex recess in the threaded end of the pin that accepts a hex key to facilitate installation (prevent fastener rotation) during torquing of the collar in clearance fit installations (see bottom of page at The pin can also be installed in interference fit holes (and the collar installed without the use of a hex key).

The S4931919 "MD" Pin ( which is identified by UG24U as a substitute part for the HL19 Hi-Lok Pin is a 6Al-4V titanium crown flush shear head threaded pin. It does not have the hex recess of the Hi-Lok pin and is intended solely for installation in interference fit installations. While there’s nothing “wrong” with this part, it is not a direct (or even necessarily good) substitution where the HL19PB has been called out…

In short:

rerig = good advice
UG24U = ???
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top