Hello,
Has anyone had experience with epoxy grout injection in cracks over 1/4" wide. There is a crack through stone masonry up to 1" wide and I'm trying to see if epoxy grout injection should be used. Most of the products I see are for up to 1/4" wide.
Thanks
 
Cracks exceeding 1/4" in width should be thoroughly cleaned and grouted. Epoxy is too expensive to fill 1" wide cracks.