While filling a bulk tank with epichlorohydrin from a road tanker, the bulk tank vented or burped and less than 50 pounds emitted. The question is how did this happen. The bulk tank was less than 3/4 full with 70,000 pounds capacity remaining. Liquid level was approximately 10 feet from full. HOW DID THIS HAPPEN?
Nitrogen on tank: 2 lbs
Pump rate: 640 lbs per minute
Nitrogen on tank: 2 lbs