Hi All,

I was wondering if someone could help me with my dilema. I am after some material data for a 70 shore hardness EPDM rubber,to run a 3d analysis of a seal in ansys workbench. I realise that many factors effect the input data but I am just trying too obtain a rough estimate of the seals behaviour and compression forces. If anyone could help it would be grately appreciated as I am having difficultly obtaining this.

Thanks
 
Hello SteveyB,

Here are the values in MPa of the two coefficients for a Mooney-Rivlin law for elastomers (EPDM).

C1(or C01)= 0.7 and C2 (or C10)= 0.2 for a 70 Shore A.

Any idea about my question, subject: Hex vs Tets / Different stress level?

BR
 