Hi all.
Im currently rebuilding an Engine. I am also slightly detailing it. I am wandering, The Exhaust manifold Nuts and studs had become very rusted and where a real pian to remove. I am wandering Will i get problems with accelerated corrision if i use Stainless Steel Studs and nuts/or stinless studs and copper nuts, When Fixed into a Cast Steel Engine block?
If so, Is there any way of preventing this?
Thanks
Steve
Im currently rebuilding an Engine. I am also slightly detailing it. I am wandering, The Exhaust manifold Nuts and studs had become very rusted and where a real pian to remove. I am wandering Will i get problems with accelerated corrision if i use Stainless Steel Studs and nuts/or stinless studs and copper nuts, When Fixed into a Cast Steel Engine block?
If so, Is there any way of preventing this?
Thanks
Steve