Mar 3, 2010 #1 AGVT Mechanical Joined Mar 3, 2010 Messages 1 Location MX I'm looking for the endurance chart cicle number vs endurance (% of yield stress). Any guide lines on where to look for it will be very useful. Bronce B150-C63000
I'm looking for the endurance chart cicle number vs endurance (% of yield stress). Any guide lines on where to look for it will be very useful. Bronce B150-C63000
Mar 3, 2010 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US I think you will find your information at this site. http://www.copper.org/ Upvote 0 Downvote