Hi All,

First and foremost, I am trying to make a dimple on a brass sheet that is 0.8mm thick. The standard to which I am making these dimples say "Deep Dimple made with a 4.8mm rod with a 5mm end radius". Can anyone explain what your understanding of this is? Maybe my understanding of End radius is wrong. Thanks for your help.

Thanks
 
First and foremost your unfortunate standard resorts to description of tool and procedure and completely ignores the final result.

Nevertheless some assumptions may be made.

"For every expert there is an equal and opposite expert"
Arthur C. Clarke Profiles of the future

 
 http://files.engineering.com/getfile.aspx?folder=cb1c0dc7-ae14-4911-b02d-e62bc61095da&file=Part2.JPG
Is there any depth requirement in your "standard"?

"For every expert there is an equal and opposite expert"
Arthur C. Clarke Profiles of the future

 
As noted, "DEEP" is relative and the required depth needs to be specified.

"Know the rules well, so you can break them effectively."
-Dalai Lama XIV
 
I searched Google for "Deep Dimple made with a 4.8mm rod with a 5mm end radius" and actually came up with the interesting document.

If this is the right one, then we have depth...

"For every expert there is an equal and opposite expert"
Arthur C. Clarke Profiles of the future

 
 http://files.engineering.com/getfile.aspx?folder=7fe9ab7f-6374-472b-ac7f-b7c19e47bccb&file=Capture.JPG
"4.8mm rod with a 5mm end radius"
Is the 4.8 the length or diameter? If the dia, would there be a point using a 5mm radius?
If the length, why call it out?

Chris, CSWA
SolidWorks 14
SolidWorks Legion
 
@ Checker Hater - Yes thats it! thats the document. And yes I forgot to mention the depth. Its 1.5mm.
 