Hello
Could you help me, how to calculate desgn stress in design temperature for bolts ?
I am praparing calculation for heat exchanger and I must use material A2-70 for bolts, but I don't have it in material library. I calculated design stress for test and 20 deg C condition (based on EN 134445-3: 2009 point 11.4.3.1 and 11.4.3.3) but I can find it for desing condition. I am preparin calculation in VVD ver 10

Thank you
Michael
 
Replies continue below

Recommended for you

What are the design conditions? In my opinion VVD is not the best program for calculating bolt stresses and a manual calculation i preferred this can be done according to EN13445-3. check also the text after table 11.4.2. hope this helps.
 
Thanks cardin

I used this text after table for calculating design stress for test condition.
Ftest = 1,5 x f 20degC
f 20degC = Rm/4
I checked values of design stress with sample bolt in VVD. These above two were ok., but f 100deg C and f 200degC were wrong, I don't find how to calculate it
 
I can remember to have read the following values for high temperature loads on these bolt.
100degC use 85% of RM (RM=700N/mm2)
200degC use 80% of RM
300degC use 70% of RM
also: A2 is austenitic and prone to SCC at temp. > 60degC (have to find the Reference again).
 
Yes I agree, I have found these values in EN 3506-1
Results are acceptable, I checek it with VVD, Thanks