Hello,
I have a doubt about the material X46Cr13 and its standard EN 10088-3.
If you check the standard 10088-3, you will see in some pages that you can perform +QT800 to the material X46Cr13. In other pages it is written +QT850 instead of +QT800. Do you know what is valid? Tha values of resistance and so on are OK? I would say the good one is +QT850, but I am not sure.
Can you help me with that please??
Thanks and regards,
I have a doubt about the material X46Cr13 and its standard EN 10088-3.
If you check the standard 10088-3, you will see in some pages that you can perform +QT800 to the material X46Cr13. In other pages it is written +QT850 instead of +QT800. Do you know what is valid? Tha values of resistance and so on are OK? I would say the good one is +QT850, but I am not sure.
Can you help me with that please??
Thanks and regards,